The effect of pre-ageing temperature and retrogression heating rate on the strength and corrosion behaviour of AA7150
Loading...
Date
Authors
Journal Title
Journal ISSN
Volume Title
Publisher
Abstract
The effects of processing condition variations in the retrogression and re-ageing (RRA) treatment of AA7150 have been investigated. The results reveal that the corrosion resistance and strength of RRA-treated samples are sensitive to the pre-ageing temperature and retrogression heating rate. With an intermediate pre-ageing temperature of 60°C and a slow retrogression heating rate of 5°C/min, RRA-treated samples can be tailored towards a good combination of both corrosion resistance and strength, owing to a smaller potential difference between grain-boundary precipitates and the matrix, and a larger volume fraction of strengthening precipitates in the matrix.