Passivation and depassivation of Si-SiO 2 interfaces with atomic hydrogen

Loading...
Thumbnail Image

Date

Authors

Zhang, Chun
Weber, Klaus
Jin, Hao

Journal Title

Journal ISSN

Volume Title

Publisher

Electrochemical Society Inc

Abstract

The influence of atomic hydrogen on the surface passivation of the Si-SiO2 interface is investigated. Inductively coupled photoconductivity decay measurements indicate an increase in carrier recombination at the surfaces following atomic hydrogen exposure, as measured by an increase in the emitter saturation current density. These defects are not thermally stable and are removed by subsequent thermal treatments above 300°C in N2. Atomic hydrogen results in the passivation of a certain fraction of thermally stable interface defects. However, the fraction of defects passivated is always slightly lower than can be achieved by exposure to molecular hydrogen. A variation in a sample temperature during atomic H exposure in the range of 25-400°C does not have a significant impact on the passivation efficiency.