Non-Destructive Evaluation of Mortar with Ground Granulated Blast Furnace Slag Blended Cement Using Ultrasonic Pulse Velocity

Loading...
Thumbnail Image

Journal Title

Journal ISSN

Volume Title

Publisher

Abstract

Non-destructive evaluation using ultrasonic pulse velocity (Vp) testing has extensive applications in the concrete industry. With advances in construction technology, the use of ground granulated blast furnace slag (GGBFS) as a partial replacement to cement in a concrete mix is growing in popularity primarily because it reduces the initial capital cost of raw materials and the associated energy costs. This paper investigates the effect of the water-to-cement (wc) ratio and the cement content replaced by GGBFS on the development with time of the ultimate compressive strength ((Formula presented.)) and the compression wave velocity (Vp) of mortar. The results showed that in the case of mortar with higher percentages of GGBFS replacement (where nucleation surfaces are more abundant), increasing wc can increase (Formula presented.) but cause a decrease in Vp. The posterior hydration process is highly dependent upon the water particles in the mixture after the first stage of hydration. After 7 days of curing, experimental results show that the (Formula presented.) of slag blended cement mix design wc ratio of 0.6 surpassed the (Formula presented.) value of an Ordinary Portland cement. A regression model correlating the (Formula presented.) and Vp of slag blended mortar is developed, which can be used to predict (Formula presented.) at concrete ages ranging from 1 day to 28 days for mixes with GGBFS percentage replacement values ranging from 15% to 45%.

Description

Publisher Copyright: © 2022 by the authors.

Citation

Loke, C K, Lehane, B, Aslani, F, Majhi, S & Mukherjee, A 2022, 'Non-Destructive Evaluation of Mortar with Ground Granulated Blast Furnace Slag Blended Cement Using Ultrasonic Pulse Velocity', Materials, vol. 15, no. 19, 6957. https://doi.org/10.3390/ma15196957